High concentration Top Diamond Clear Coat spray Pain with HT Basecoat - Product
Place of Origin : Guangzhou,China
Delivery Time : 5-10 Days
Product Description
High concentration Top Diamond Clear Coat spray Pain with HT Basecoat
Clear Top Coat Pain, 9000 Diamond Clear Coat, High concentration, high gloss varnish, solid content, enduring gloss
Quick Detail:
- - - -
Product Type | High concentrated , high gloss clear coat with high solid . No change in gloss for a long time , high build , excellent chemical resistant ; The best car refinishing effect in combination with Diamond Hardener |
Subsrate | Surface coated with HT B
Physical Specification
Other Specification :
High Concentration Top Diamond Clear Coat Spray Pain With HT Basecoat
Clear Top Coat Pain, 9000 Diamond Clear Coat, High Concentration, High Gloss Varnish, Solid Content, Enduring Gloss
Quick Detail:
- - - -
Product Type | High Concentrated , High Gloss Clear Coat With High Solid . No Change In Gloss For A Long Time , High Build , Excellent Chemical Resistant ; The Best Car Refinishing Effect In Combination With Diamond Hardener |
Subsrate | Surface Coated With HT Basecoat |
Blending Ratio | 20
HT-9000 Diamond Clear Coat 100parts
PU-900 Diamond Slow Drying Hardener 50parts
X-2Standar Thinner 15-25parts |
20-28
HT-9000 Diamond Clear Coat 100parts
PU-900 Diamond Standard Hardener 50parts
X-2/X-3Thinner 15-25parts |
28
HT-9000 Diamond Clear Coat 100parts
PU-900 Diamond Slow Drying Hardener 50parts
X-4Extra Slow Thinner 15-25parts |
Pot Life | Diamond Standard Hardener : 3hours , 20 |
Spray Methods | 2-3layers , 4060m Thickness , The Volatile Time Is 5-10mins |
Spray Gun Ressure | Gravity Feed Spray Gun 1.2-1.5mm 3.0-5.0kg/cm2
Suction Spray Gun 1.4-1.7mm 3.0-5.0kg/cm2 |
Drying Time | Temperature | Anti-dust Time | Tack Free Time | Assembly Time | Completely Dry |
20 | 45mins | 2-3hours | 10huors | 7days |
60 | 5mins | 10mins | 30mins | 60mins |
Shelf Life | 18months If Stored In Its Original Sealed Cans At 20 |
Packing | 1liter , 4liter Or 5 Liter Can |
- - - -
Precautions:
(1) If The Air Pressure Is Too Low, The Spray Viscosity Is Too Big And Each Spray Coat Is Too Thick, Then The Spray Effect Wont Be Ideal.
(2) As The Two-component Paint Would React With Water, There Should Never Be Any Water Content In All Equipment, Containers And Spray Guns.
(3) The Two-component Baking Paint Hardener Contains Isocyanic Acid That Irrita