CAS No. 31570-04-4 Phenolic Antioxidants ANTIOXIDANT 168 , IRGAFOS 168 - Product
Place of Origin : Qingdao,China
Delivery Time : Prompt
Product Description
1,Name:FUNDAOX 168
2,Appearance:White crystalline powder
3,CAS No.:31570-04-4
4,Fuction:Low volatility, Protects polymers
5,Use:stabilize polyesters, polycarbonates, polyamides, polystyrene, and elastomers. Use levels can range from 0.10 to 0.80% based on the polymer.
CAS No. 31570-04-4 Phenolic Antioxidants ANTIOXIDANT 168 , IRGAFOS 168
Description:
FUNDAOX 168 is a hydrolytically stable phosphate processing stabilizer. As a secondary Fundaox, it reacts during processing with hydr
Physical Specification
Other Specification : 1,Name:FUNDAOX 168
2,Appearance:White Crystalline Powder
3,CAS No.:31570-04-4
4,Fuction:Low Volatility, Protects Polymers
5,Use:stabilize Polyesters, Polycarbonates, Polyamides, Polystyrene, And Elastomers. Use Levels Can Range From 0.10 To 0.80% Based On The Polymer.
CAS No. 31570-04-4 Phenolic Antioxidants ANTIOXIDANT 168 , IRGAFOS 168
Description:
FUNDAOX 168 Is A Hydrolytically Stable Phosphate Processing Stabilizer. As A Secondary Fundaox, It Reacts During Processing With Hydroperoxides Formed By Autoxidation Of Polymers Preventing Process Induced Degradation And Extending The Performance Of Primary Fundaoxs.
Applications:
FUNDAOX 168 Can Be Used As A Processing Stabilizer In Polymers To Help Control Color Degradations And Melt Flow.
FUNDAOX 168 Is Particularly Useful In The Stabilization Of Polyolefins, EVA, Olefinic Copolymers When Used In Conjunction With A Phenolic Fundaox.
FUNDAOX 168 Can Also Be Used To Stabilize Polyesters, Polycarbonates, Polyamides, Polystyrene, And Elastomers. Use Levels Can Range From 0.10 To 0.80% Based On The Polymer.
Specifications:
- - - -
Appearance: | White Crystalline Powder |
Melting Point: | 183-187C |
Content: | 99% Min. |
Volatile(105C,2h): | 0.3%Max. |
Light Transmittance: (10g/100ml Toluene) | 98% Min. @ 425nm 98% Min. @ 500nm |
Solute In Toluene (10g/100ml) | Clear |
- - - -
Competitive Advantage:
# # Low Volatility And Is Particularly Resistant To Hydrolysis.
# Protects Polymers Which Are Prone To Oxidation, During The Processing Steps From Molecular Weight Change And Prevents Discoloration.
# Provides Storage Stability And Give The Polymer Long Term Protection Against Thermo-oxidative Degradation.
# Comprised In Phenol Free Systems With Other Appropriate Stabilizers Addresses Specific Stabilization Requirements.
#