HIGH SPEED STEEL M35/SKH55
Anneal temperature: 840-860
Relief annealing temperature: 720-760
Hardening temperature: 1200-1235
Hardening medium: salt bath under 600,aslo use oil cooling or air cooling
Normal temper temperature: 540-560
RC Rockwell Hardness after hardening and tempering: 64-67
Characteristic:Tungsten-molybdenum high speed steel, better performance of hardness, red hardness, thermoplasticity, machinability than W6Mo5Cr4V2 . Weak in impact toughness and intensity.